Analisa Pengaruh Casting Speed dan Superheat Terhadap Cacat Permukaan Slab Baja Grade 1A0804

Herdi Susanto

Abstract


Increasing the life of the continuous casting machine causes a defect on the surface of the steel slab, it takes some corrective measures for the casting process, such as by redefining and updating the standard operating parameters that influence the casting process with a review of the surface defects. This research was conducted at the Division of Steel Slab Plant II PT. Krakatau Steel using casting machine kontiyu Low head machine with a straight mold, angle and transverse crack at grade steel slab 1A0804. The result showed the operating parameters are better at ≤ 1.30 casting speed <1.35 m/min and 250 <superheat ≤ 300 C. From these results it can be concluded that the standard operating parameters of continuous casting to casting speed of 1.4 m / min is important to be updated and superheat 300C can still be used

Keywords : steel 1A0804, casting speed, superheat, angle crack, transverse crack


Full Text:

PDF

References


. Anonym, 1993, Technical Documentation, Steel Slab Plant Extention PT. Krakatau Steel, PT. Krakatau Engineering Corporation, dan Voest Alfine Industrieanlagenbau (VAI). Item No. 3.05.01.

. Anonym, 1999, Standard Operation Procedure, Refer No. 041/V/99, SSP1/SSP2 PT. Krakatau Steel.

. Anonym, 2002, Modul Pelatihan Metalurgi Proses, PT. Krakatau Steel.

. R. E. Smallman, 1991, Metalurgi Fisik Modern PT. Gramedia Pustaka Utama, Jakarta.

. W.O. Alexander, et al, 1991, Dasar Metalurgi Untuk Rekayasawan, PT. Gramedia Pustaka Utama, Jakarta.